Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527-1/-2 |
DSM Akulon® S223-PG6U (Dry) 33% Glass Reinforced, Impact Modified Nylon 66 (North America)
(discontinued **)& Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ASTM D638 |
Plenco 7527 Phenolic, Nodular, Injection Molded
(discontinued **) Single-Stage Phenolic. PLENCO 07527 is a flock cotton and mineral filled resole phenolic molding compound.Information supplied by Plenco |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V25 Natural B PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, specially stabilized to improve its resistance to oils and greases, for injection molding.Available in: EuropeProduct Applications: Thi.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527 |
Solvay Technyl® A 218 V35 Nylon 66, 35% Glass Fiber, EH50 Polyamides PA66, reinforced with 35% of glass fiber, heat stabilized, for injection molding.Technyl A 218 V35 is used in all sectors of industry, offering an excellent combination between thermal an.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36R PA6.12 (Europe-Africa-Middle East) Internally lubricated PA6.12, containing Glass Fiber and PTFE |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON SE002Z PA 12 (Asia Pacific) LNP* Stat-kon* SE002Z is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Asia Pacific) LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermotuf PF007IX2 PA 6 (Europe-Africa-Middle East) LNP * THERMOTUF* PF007IX2 is a compound based on PA 6 resin containing Glass Fiber. Added features include: High Impact.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527-1/-2 |
Unitika BV2120G30 PA66, 30% Glass Fiber Reinforced, Flame Retardant, Conditioned Information provided by Unitika Ltd. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ASTM D638 |
Plenco 5482 Phenolic, Granular, Injection Molded PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ASTM D638 |
Plenco 5482 Phenolic, Granular, Transfer Molded PLENCO 05482 is an organic reinforced phenolic molding compound formulated with graphite to improve the abrasion resistance. 05482 is available in black and brown. 05482 is not recommended for elect.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ASTM D638 |
Plenco 2571 Phenolic, Granular, Injection Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-30 HM PA6-GF30 Product description: Grilon BG-30 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 30% glass fibers. Grilon BG-30 HM has the following important prop.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GV 30 HW 30% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® FR95G25V0NH NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 ZYTEL FR95G25V0NH NC010 is 25% glass fiber reinforced flame retardant polyamide halogen and red phosphorous free with high flow and excellent long t.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam AFR450X2 PA66, 25% Glass Filled, Injection Molded AFR450X2 is a Red Phosphorous, Flame Retardant, 25% Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive su.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ASTM D638 |
BLUESTAR 101G30 PBT, 30% Glass Filled Typical Applications: Appliances, molded partsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527-1/-2 |
DSM Arnite® TZ6 280 PBT-(GF+GB)40 20% Glass Reinforced, 20% Glass Beads Reinforced |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | |
LATI Latimass 82-03 D110 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Tensile Modulus | 8.70 GPa | 1260 ksi | ISO 527-1/-2 |
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT Description: injection-molding grade with 30% glass-fibers; for rigid and dimensionally stable technical parts with increased requirements on hydrolysis resistance. For example automotive connectors.. |