Polymer Property : Heat of Fusion = 48.0 J/g Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 40.0 - 48.0 J/g
17.2 - 20.6 BTU/lb
80°C to end of melting; ASTM D3418
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 5130 PVDF has an ultra high viscosity ideal for its usage in lithium batteries.Additional Information: Intrinsic Viscosity: 0.27 - 0.37 l/gInformation provided by Solvay Specialty Polymers.