Polymer Property : Density = 0.0643 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.75 - 1.78 g/cc
0.0632 - 0.0643 lb/in³
ISO 1183
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 5130 PVDF has an ultra high viscosity ideal for its usage in lithium batteries.Additional Information: Intrinsic Viscosity: 0.27 - 0.37 l/gInformation provided by Solvay Specialty Polymers.
Density 1.45 - 1.78 g/cc
0.0524 - 0.0643 lb/in³
Average value: 1.57 g/cc Grade Count:144
Overview of materials for Nylon 66, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Density 1.22 - 1.78 g/cc
0.0441 - 0.0643 lb/in³
Average value: 1.45 g/cc Grade Count:114
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Density 1.75 - 1.78 g/cc
0.0632 - 0.0643 lb/in³
ISO 1183
Solvay Specialty Polymers Solef® 5120 Polyvinylidene Fluoride (PVDF)
Solef® 5120 PVDF is a medium viscosity grade that gives improved adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Medium ViscosityUses: Batteries; BinderAdditional Prope..
Density 1.75 - 1.78 g/cc
0.0632 - 0.0643 lb/in³
ISO 1183
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)
Solef® 5130 PVDF is an ultra high viscosity grade that gives the best adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Ultra High ViscosityUses: Batteries; BinderAdditio..
Density 1.73 - 1.78 g/cc

@Temperature 22.0 - 24.0 °C
0.0625 - 0.0643 lb/in³

@Temperature 71.6 - 75.2 °F
Shandong Dongyue Shenzhou New Material Co Fluorocarbon Solvent
Conformable with: Q/DYS 012-2007Fluorocarbon solvent is a mixture of perfluorocarbon circular ether. It is a colorless transparent liquid, odorless, nontoxic and uninflammable. It is unsoluble in ..
Density 1.68 - 1.78 g/cc
0.0607 - 0.0643 lb/in³
Molding; IS 867-1963
Amity Thermosets ATE 183 M Phenolic Molding Mica and organic Filler, Compression Molded
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl..
Density 1.71 - 1.78 g/cc
0.0618 - 0.0643 lb/in³
Molded
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound
BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro..
Density 1.68 - 1.78 g/cc
0.0607 - 0.0643 lb/in³
Molding; IS 867-1963
Amity Thermosets ATE 183 Phenolic Molding Mica and organic Filler, Compression Molded
Characteristics:Electric low loss Low water absorption Low shrinkage Heat stableGlossy surface finishVery good mouldabilityGood electrical insulationGood chemical resistantColor-blackMedium flowAppl..
Density 1.26 - 1.78 g/cc
0.0455 - 0.0643 lb/in³
Average value: 1.62 g/cc Grade Count:36
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..