Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DMTA |
Solvay Specialty Polymers Solef® 3208/0150 Anti-friction PVDF Compound
(discontinued **) Key features of this grade: Anti-friction, Formulated. Recommended processing is injection. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
Mallard Creek Polymers TYLAC® 873 Nitrile Emulsion Tylac® 873 is a carboxylated acrylonitrile-butadiene copolymer latex. Features: good resistance to oil, grease and solvent, compatible with anionic asphalt emulsions, broadens the temperature ran.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
Seals Eastern 5241 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
Seals Eastern 5242 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
Seals Eastern 5243 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
Seals Eastern 7065 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
Seals Eastern 7282 Neoprene / Chloroprene UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: MembranesAddition.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF) Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
Solvay Specialty Polymers Solef® 5120 Polyvinylidene Fluoride (PVDF) Solef® 5120 PVDF is a medium viscosity grade that gives improved adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Medium ViscosityUses: Batteries; BinderAdditional Prope.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
Styron XZ 91945.00 Functionalized SB Performance Features: Very soft tacky film, self cross-linking, good pigment acceptanceApplications: Performance CoatingsEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
Wanhua Chemical Wanthane® WHT-8195 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -40.0 - -30.0 °C | -40.0 - -22.0 °F | |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
Lubrizol Estane® 2103-84AEN Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Contains UV Stabilizer, NSF Standard 61 certifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pelletha.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | Pellet sample |
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 460 Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Broad molecular weight distribution, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, .. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D3418 |
Wanhua Chemical Wanthane® WHT-1185 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
Lubrizol Estane® 58437 Thermoplastic Polyurethane Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |