Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 245 MPa @Strain 0.200 %, Temperature 540 °C |
35500 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Tensile Strength, Yield | 245 MPa @Strain 0.200 %, Temperature 650 °C |
35500 psi @Strain 0.200 %, Temperature 1200 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Tensile Strength, Yield | >= 245 MPa @Strain 0.200 %, Temperature 21.1 °C |
>= 35500 psi @Strain 0.200 %, Temperature 70.0 °F |
|
H.C. Starck Ultra 76 Alloy (Ta 2.5%W) Benefits: Significantly improved corrosion resistance in HCl and H2SO4 acids.Minimized hydrogen embrittlement rates compared to standard NRC®76Up to 100 times lower in HCl acidUp to 10 times low.. |
|||
Tensile Strength, Yield | 245 MPa | 35500 psi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 5950 HFFR Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 5950 HFFR is a halogen-free, flame retardant (UL-94 V0 at 0.4 mm), highly reinforced polyamide material specifically formulated for high strength and stiffness applications where good impa.. |
|||
Tensile Strength, Yield | 245 MPa | 35500 psi | ISO 527-2 |
Solvay Specialty Polymers Kalix® 9950 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 9950 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties and excellent surface .. |
|||
Tensile Strength, Yield | 245 MPa | 35500 psi | ISO 527-2 |
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Dry) Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used .. |