Material Notes:
Description: INDURE™ X190 engineered polyolefin material is designed for large, molded-in-color automotive exterior applications that require good scratch and mar characteristics, high stiffness, and low coefficients of linear thermal expansion (CLTE). Applications: Exterior ornamentation, bezels, luggage rack components. Information provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792B
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
as molded; ISO 294
Melt Flow 10 - 12 g/10 min
10 - 12 g/10 min
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.8 MPa
3310 psi
150x10x4 mm specimen, 50 mm/min; ASTM D638
Flexural Modulus 1.90 GPa
276 ksi
80x10x4 mm specimen, 2 mm/min; ASTM D790
Impact Test 16.0 J
11.8 ft-lb
multiaxial, 2.2 m/s; ASTM D3763
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature 20.0 °C
33.3 µin/in-°F

@Temperature 68.0 °F
modified; ASTM D696