Material Notes:
Description: INDURE™ E1500 HG is a thermoplastic olefinic elastomer (TPO) designed for high-gloss thermoformed applications where excellent gloss retention after forming is required. This material is available in both UV-stabilized and non-UV-stabilized variants. The material is designed for use as a coextrusion cap layer with other extrusion-grade TPOs from Solvay Engineered Polymers. Applications: High-gloss, thermoformed interior and exterior parts. Information provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792B
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
IV 2 in/min; ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 1.01 GPa
146 ksi
1% SEC, 0.05 in/min; ASTM D790
Izod Impact, Notched 0.395 J/cm
0.740 ft-lb/in
CB; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 73.9 °C
165 °F
ASTM D648
Optical Properties Metric English Comments
Gloss >= 85 %
>= 85 %
60°C Gardner Gloss, smooth sheet, after forming; ASTM D523
>= 85 %
>= 85 %
60°C Gardner Gloss, smooth sheet, before forming; ASTM D523