Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.01 GPa | 146 ksi | 1% SEC, 0.05 in/min; ASTM D790 |
Solvay Engineered Polymers INDURE™ E1500 HG TPO
(discontinued **) Description: INDURE™ E1500 HG is a thermoplastic olefinic elastomer (TPO) designed for high-gloss thermoformed applications where excellent gloss retention after forming is required. This material.. |
|||
Flexural Modulus | 1.01 GPa | 146 ksi | 1% SEC, 0.05 in/min; ASTM D790 |
Solvay Engineered Polymers INDURE™ E1600 TPO
(discontinued **) Description: INDURE™ E1600 is a thermoplastic olefinic elastomer (TPO) designed for high-gloss thermoformed applications where excellent gloss retention after forming is required. This material is.. |
|||
Flexural Modulus | 1.01 GPa | 146 ksi | 12.5 mm/min; ASTM D790 |
LyondellBasell Alathon® M4855 High Density Polyethylene, Injection Molding Grade ALATHON M4855 is a high density copolymer for use in injection molding applications. It exhibits excellent impact, warp and environmental stress crack resistance. Typical applications for M4855X01 a.. |
|||
Flexural Modulus | 1.01 GPa | 146 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem GF 5250 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.01 GPa | 146 ksi | 1% secant, 0.05 in/min.; ASTM D790 |
ExxonMobil PP7035E4 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |
|||
Flexural Modulus | 1.01 GPa | 146 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow DMDB-7950 NT 7 High Density Polyethylene Resin DOW DMDB-7950 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as roll-out trash carts and other large parts with short mo.. |
|||
Flexural Modulus | 1.01 GPa | 146 ksi | |
Dow HDPE 08454N High Density Polyethylene DOW HDPE 08454N resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and toughness, with good stiffness. This resin has good processability over a wi.. |
|||
Flexural Modulus | 1.01 GPa | 146 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
Dow UNIVAL™ DMDA-6320 NT 7 High Density Polyethylene Resin (HDPE) Low swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6320 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package household.. |
|||
Flexural Modulus | 1.01 GPa | 146 ksi | |
Dow HDPE 65053N High Density Polyethylene DOW HDPE 65053N resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and rigidity with high impact strength. This resin has excellen.. |
|||
Flexural Modulus | 1.01 GPa | 146 ksi | ISO Data |
BASF Ultramid® 8202CQ PA6 (Conditioned) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
Flexural Modulus | 1.01 GPa | 146 ksi | ASTM D790 |
Multibase Multi-Flam™ 0801 PP Polypropylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingExtrusionCoextrusionUses:TubingPipingFurnitureInformation provided by Multibase |