Silikony Polskie Silpasta P Silicone Paste

Category Fluid , Lubricant , Silicone Base
Manufacturer Silikony Polskie
Trade Name Silpasta
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Silikony Polskie Silpasta P Silicone Paste.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A consistency of hard VaselineTo improve thermal conduction in electrotechnical and mechanical devices.
Physical Properties Metric English Comments
Density 2.00 g/cc
0.0723 lb/in³
pH 6.5 - 7.5
6.5 - 7.5
Storage Temperature -40.0 - 50.0 °C
-40.0 - 122 °F
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Dielectric Loss Index 0.050

@Frequency 100 Hz
0.050

@Frequency 100 Hz
Descriptive Properties Value Comments
Hygienic Certificate PZH HK/B/0829/02/2005