Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | -40.0 - 50.0 °C | -40.0 - 122 °F | |
Silikony Polskie Silpasta A Silicone Paste Vaseline consistency, slightly thixotropicAntiadhesive agent used in thermoplastic and thermosetting processing to paste ground joints, rubber gaskets, etc. |
|||
Storage Temperature | -40.0 - 50.0 °C | -40.0 - 122 °F | |
Silikony Polskie Silpasta E Silicone Paste Vaseline consistency, thixotropicElectric insulation to paste insulators, conductor connection, cable boxes in environment of high humidity or dustiness. |
|||
Storage Temperature | -40.0 - 50.0 °C | -40.0 - 122 °F | |
Silikony Polskie Silpasta EM Silicone Paste Vaseline consistency, thixotropicElectric insulation for mechanical application of protective layers on electric devices and connections. |
|||
Storage Temperature | -40.0 - 50.0 °C | -40.0 - 122 °F | |
Silikony Polskie Silpasta P Silicone Paste A consistency of hard VaselineTo improve thermal conduction in electrotechnical and mechanical devices. |
|||
Storage Temperature | -40.0 - 50.0 °C | -40.0 - 122 °F | |
Silikony Polskie Silpasta R Silicone Paste Semi-liquid consistencyLubricant agent during assembly of PVC pipelines. |
|||
Storage Temperature | -40.0 - 50.0 °C | -40.0 - 122 °F | |
Silikony Polskie Silpasta Z Silicone Paste A consistency of hard VaselineLubricating agent to dampen vibrations in transmission gears and other mobile element made of plastic. |