Material Notes:
KE-1950-10 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy pumping through most injection molding systems.FeaturesRapid cure time at elevated temperatureLong pot life at room temperatureApplicationsO-ringsDiaphragmsCappingRubber rollersConnector packingsOther electrical partsInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
Viscosity 60000 cP
60000 cP
A
60000 cP
60000 cP
B
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 13
13
Tensile Strength 3.90 MPa
566 psi
Elongation at Yield 700 %
700 %
100% Modulus 0.000207 GPa
0.0300 ksi
Tear Strength 10.0 kN/m
57.1 pli
Compression Set 8.0 %

@Temperature 200 °C,
Time 14400 sec
8.0 %

@Temperature 392 °F,
Time 4.00 hour
12 %

@Temperature 150 °C,
Time 3600 sec
12 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 120 °C
0.0833 hour

@Temperature 248 °F
Press Cure
60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
Post Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 38
T10 (302°F, ODR)
86
T90 (302°F, ODR)
Regulatory Testing Class VI, FDA