Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.023 cm/cm | 0.023 in/in | Flow; ISO 294-4 |
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE) Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr.. |
|||
Linear Mold Shrinkage | 0.023 - 0.027 cm/cm | 0.023 - 0.027 in/in | ASTM D955 |
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
Linear Mold Shrinkage | 0.023 cm/cm @Thickness 80.0 mm |
0.023 in/in @Thickness 3.15 in |
sheet; ASTM D4894 |
3M Dyneon™ TFM™ 4105 Modified PTFE, 25% Glass Fiber Filled
(discontinued **) Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon. |
|||
Linear Mold Shrinkage | 0.023 cm/cm @Thickness 80.0 mm |
0.023 in/in @Thickness 3.15 in |
sheet; ASTM D4894 |
3M Dyneon™ TF 4215 PTFE 25% Electrocarbon Filled
(discontinued **) Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon. |
|||
Linear Mold Shrinkage | 0.023 cm/cm | 0.023 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-10A/B Elastomer KE-1950-10 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Linear Mold Shrinkage | 0.023 cm/cm | 0.023 in/in | ASTM D955 |
Teknor Apex Monprene® MP 1085 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.023 cm/cm | 0.023 in/in | ASTM D955 |
Teknor Apex Monprene® MP-1644L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.023 cm/cm | 0.023 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2004-10A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Linear Mold Shrinkage | 0.023 cm/cm | 0.023 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2004-5A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Linear Mold Shrinkage | 0.023 cm/cm | 0.023 in/in | |
Shin-Etsu Silicones LIMSâ„¢ KE2090-40AB Elastomer KE-2090-40 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo.. |
|||
Linear Mold Shrinkage | 0.023 cm/cm | 0.023 in/in | |
Polyram RamSter PF100 PBT, General Purpose General purpose, high viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Linear Mold Shrinkage | 0.023 cm/cm | 0.023 in/in | ASTM D955 |
Teknor Apex Monprene® MP-2357-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Linear Mold Shrinkage | 0.023 cm/cm | 0.023 in/in | |
Polyram RamSter PF201 PBT, General Purpose, Medium Viscosity General purpose, medium viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |