Physical Properties Metric English Comments
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
Flow; ISO 294-4
PolyOne Versalloy™ HC 9220-80 Thermoplastic Elastomer (TPE)
Versalloy™ HC 9220-80 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical gr..
Linear Mold Shrinkage 0.023 - 0.027 cm/cm
0.023 - 0.027 in/in
ASTM D955
Polymer Resources TP-IM1 Polybutylene Terephthalate, Low Temperature Impact Modified
Polybutylene Terephthalate, Low Temperature Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor..
Linear Mold Shrinkage 0.023 cm/cm

@Thickness 80.0 mm
0.023 in/in

@Thickness 3.15 in
sheet; ASTM D4894
3M Dyneon™ TFM™ 4105 Modified PTFE, 25% Glass Fiber Filled  (discontinued **)
Type II PTFE. Applications include valve seats, bearings, seals/gaskets, moldings, piston rings.Data provided by Dyneon.
Linear Mold Shrinkage 0.023 cm/cm

@Thickness 80.0 mm
0.023 in/in

@Thickness 3.15 in
sheet; ASTM D4894
3M Dyneon™ TF 4215 PTFE 25% Electrocarbon Filled  (discontinued **)
Applications include bearings, seals/gaskets, packings, piston rings.Data provided by Dyneon.
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
Shin-Etsu Silicones LIMSâ„¢ KE1950-10A/B Elastomer
KE-1950-10 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy ..
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
ASTM D955
Teknor Apex Monprene® MP 1085 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
ASTM D955
Teknor Apex Monprene® MP-1644L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
Shin-Etsu Silicones LIMSâ„¢ KE2004-10A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
Shin-Etsu Silicones LIMSâ„¢ KE2004-5A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
Shin-Etsu Silicones LIMSâ„¢ KE2090-40AB Elastomer
KE-2090-40 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
Polyram RamSter PF100 PBT, General Purpose
General purpose, high viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
ASTM D955
Teknor Apex Monprene® MP-2357-L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage 0.023 cm/cm
0.023 in/in
Polyram RamSter PF201 PBT, General Purpose, Medium Viscosity
General purpose, medium viscosity PBT for injection molding applicationsInformation provided by Polyram Ram On Ind.