Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 3.90 MPa | 566 psi | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-10A/B Elastomer KE-1950-10 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Tensile Strength | 3.90 MPa | 566 psi | |
Shin-Etsu Silicones KE-1831 Silicone, RTV Adhesive/Sealant Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tensile Strength | 3.90 MPa | 566 psi | 500 mm/min, measured parallel to flow; ISO 37 |
AlphaGary Evoprene™ LF 6151 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tensile Strength | 3.90 MPa | 566 psi | ISO 37 |
AlphaGary Evoprene™ G 966 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |