Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samyang Tribit® 1500G30K PBT, Reinforced Impact

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Samyang
Trade Name Tribit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samyang Tribit® 1500G30K PBT, Reinforced Impact.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G30K is a reinforced, impact grade.Applications: Connectors (insulation characteristics)Information provided by Samyang.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.0020 - 0.012 cm/cm
0.0020 - 0.012 in/in
ASTM D955
Melt Flow 38 g/10 min

@Load 2.16 kg,
Temperature 250 °C
38 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength 98.1 MPa
14200 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 137 MPa
19900 psi
ASTM D790
Flexural Modulus 5.39 GPa
782 ksi
ASTM D790
Izod Impact, Notched 0.785 J/cm

@Thickness 3.17 mm
1.47 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 30.0 µm/m-°C
16.7 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 230 °C
446 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
419 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.2
3.2
ASTM D150
Dielectric Strength 25.0 kV/mm
635 kV/in
ASTM D149
Dissipation Factor 0.020
0.020
ASTM D150
Arc Resistance 130 sec
130 sec
ASTM D495