Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP2122G15VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 0.785 - 9.08 J/cm | 1.47 - 17.0 ft-lb/in | Average value: 5.97 J/cm Grade Count:64 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose Feature: Injection Molding, PA66+GF20%, General PurposeApplication: Automotive PartsCAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2339B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPET® KP133G45 FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP212G30VO G/F Reinforced & Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP2300R PBT+GF30% Description: Injection Molding, PBT+GF30%, Anti-HydrolysisApplication: E&E (Speed Nut & Body)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.785 J/cm @Temperature 23.0 °C |
1.47 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC M1315 Polypropylene Impact Copolymer Features: SEETEC M1315 is a heterophasic polypropylene copolymer for compression molding caps, especially SACMI machines. SEETEC M1315 exhibits an excellent stiffness, a high impact strength, a high.. |
|||
Izod Impact, Notched | 0.784 J/cm | 1.47 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® SM240 Polypropylene impact copolymer Titanpro® SM240 is a high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet .. |
|||
Izod Impact, Notched | >= 0.785 J/cm @Thickness 6.35 mm |
>= 1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PET 9030-104E 30% Glass/Mineral Filled Product Description: PET glass 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent wear.. |
|||
Izod Impact, Notched | >= 0.785 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 1.47 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN2101F PC+GF10%, Halogen Free, Flame Retardant, Heat Resistance Description: Injection Molding, PC+GF10%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov.. |
|||
Izod Impact, Notched | 0.785 J/cm @Temperature 23.0 °C |
1.47 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUTENE-H ME6000 HDPE Description: LUTENE-H ME6000 is mainly intended for injection molding of crates. It has excellent mechanical properties and high impact strength.Applications: Transport and stacking crates, bottle c.. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | |
Shinil Chemical SHINCON PC Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm |
1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® XP-2130A PPS Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4017 ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4020H ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1101 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4020H ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Tribit® 1500G30K PBT, Reinforced Impact Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G30K is a reinforced, impact grade.Appl.. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 6.35 mm |
1.47 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® XP-2130A PPS Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | |
Zylog Hipolyene® 2530 DW Thermoplastic Polyolefin & PP Compound Information provided by Zylog Plastalloys Pvt. Ltd. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T889G2 PBT, 20% Glass Fiber |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
E-Polymers TEKAFIN® PH70G1 HIPP + 10% Glass Fiber Reinforced Scratch Resistance Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® JN930 PPE+PA66 30% Glass Fiber Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV3020 Polyformaldehyde |
|||
Izod Impact, Notched | 0.785 - 6.00 J/cm | 1.47 - 11.2 ft-lb/in | Average value: 3.05 J/cm Grade Count:40 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 0.785 - 0.981 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.47 - 1.84 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Samyang Triel® 5652EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5652EM is an extrusion grade.Information provided by Samyang. |