Polymer Property : Flexural Modulus = 5.39 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 5.39 GPa
782 ksi
DIN 53452; ASTM D790
Kolon KOLEFIN® KO133GM40 M/F Reinforced Polypropylene
KOLEFIN® has excellent mechanical properties and its cost is lower than other engineering plastics. KOLEFIN® is widely used in the automotive industry and business applications.Good mechanica..
Flexural Modulus 5.39 GPa

@Thickness 3.20 mm
782 ksi

@Thickness 0.126 in
15mm/min; ASTM D790
LG Chemical LUCON PS4200 ABS+CF
Description: Injection Molding, ABS+CF, Electrostatic Dissipation, Good Dimensional Stability, Low WarpageApplication: IC TrayCAS No. 9003-56-9, 12001-26-2 and 7440-44-0Information provided by LG Ch..
Flexural Modulus 5.39 GPa
782 ksi
ASTM D790
Kotec Carbotex KG-20F10 Polycarbonate, Wear Resistant, 20% Glass Fiber Reinforced
Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Non-frictionApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation p..
Flexural Modulus 5.39 GPa

@Thickness 3.20 mm
782 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOY GP2200 PC+GF20%, Heat Resistance
Description: Injection Molding, PC+GF20%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Flexural Modulus 5.39 GPa
782 ksi
ASTM D790
Gromax PBT 4115-104D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Flexural Modulus 5.39 GPa
782 ksi
DIN 53452; ASTM D790
Kolon KOPA® KN178MT40 M/F Reinforced Nylon 6
KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr..
Flexural Modulus 5.39 GPa

@Thickness 3.20 mm
782 ksi

@Thickness 0.126 in
10mm/min; ASTM D790
LG Chemical LUPOS GP2200 ABS+GF20%, General Purpose
Feature: Injection Molding, ABS+GF20%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical
Flexural Modulus 5.39 GPa
782 ksi
ASTM D 790
SABIC Innovative Plastics Valox® DR48M PBT (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
Flexural Modulus 5.39 GPa
782 ksi
Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite Engine Cover
SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using..
Flexural Modulus 5.39 GPa
782 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® HF-3200H PC, Glass Filled High Impact
Information provided by Samsung Cheil Industries.
Flexural Modulus 5.39 GPa
782 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 5.39 GPa
782 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® HF-3200H PC, Glass Filled High Impact
Information provided by Samsung Cheil Industries.
Flexural Modulus 5.39 GPa
782 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® HN-3203G PC, Glass Filled FR
Information provided by Samsung Cheil Industries.
Flexural Modulus 5.39 GPa
782 ksi
ASTM D790
Samyang Tribit® 1500G30K PBT, Reinforced Impact
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G30K is a reinforced, impact grade.Appl..
Flexural Modulus 5.39 GPa
782 ksi
ASTM D790
Samyang Tribit® 1550GN15 PBT Alloy, Reinforced Flame Retardancy
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN15 is a reinforced, flame retardant (..
Flexural Modulus 5.39 GPa
782 ksi
ASTM D790
Samyang Tribit® 1551GN15 PBT, Reinforced Flame Retardancy
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN15 is a reinforced, flame retardant g..
Flexural Modulus 5.39 GPa
782 ksi
ASTM D790
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Flexural Modulus 5.39 GPa
782 ksi
ASTM D790
Gromax PBT 4115-201D 15% Glass Fiber Filled
Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Flexural Modulus 5.39 GPa
782 ksi
ASTM D790
PlastxWorld CEVIAN® B5523 15% GF PBT/ABS Alloy
Glass fiber reinforced and flame retarded PBT/ABS alloy.Information provided by PlastxWorld Inc.
Flexural Modulus 5.39 GPa

@Thickness 3.20 mm
782 ksi

@Thickness 0.126 in
1.3mm/min; ASTM D790
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose
Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical