Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 30% Glass Filled
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Melt Flow 6.0 g/10 min

@Load 10.0 kg,
Temperature 280 °C
6.0 g/10 min

@Load 22.0 lb,
Temperature 536 °F
ASTM D1238
Ash 30 %
30 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Yield 118 MPa
17100 psi
5 mm/min; ASTM D638
Flexural Strength 157 MPa
22800 psi
2.8 mm/min; ASTM D790
Flexural Modulus 7.26 GPa
1050 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 148 °C

@Thickness 6.40 mm
298 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 140 °C
284 °F
B/50; ISO R306