Mechanical Properties Metric English Comments
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Izod Impact, Notched 1.08 J/cm

@Temperature -30.0 °C
2.02 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
Izod Impact, Notched 1.08 J/cm

@Temperature -30.0 °C
2.02 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Asia Pacific)
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
Izod Impact, Notched 1.08 J/cm

@Temperature -30.0 °C
2.02 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1930 PC Copolymer (Europe-Africa-Middle East)
55 MFR LEXAN High Flow Ductile Copolymer, Natural color only
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Polimersan Plastics POLITEF® (PTFE) with 60% Bronze
As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv..
Izod Impact, Notched 1.08 J/cm

@Temperature -30.0 °C
2.02 ft-lb/in

@Temperature -22.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1910 PC Copolymer
55 MFR LEXAN High Flow Ductile Copolymer, Natural colors only
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Izod Impact, Notched 1.08 - 1.40 J/cm
2.02 - 2.62 ft-lb/in
Average value: 1.29 J/cm Grade Count:4
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
Izod Impact, Notched 1.08 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.02 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Kolon KOPA® KN333G30CRN G/F Reinforced Nylon 66
Oil resistantApplications Surge tanksInformation provided by API-Kolon.
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Kolon KOPA® KN333G30HS G/F Reinforced Nylon 66
High thermal resistant, high strength, dimensionally stableApplications Transmission gear supportersInformation provided by API-Kolon.
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Kolon KOPA® KN333G35CRBK G/F Reinforced Nylon 66
EG-resistant, high strength, dimensionally stableApplications Coolant temperature control partsInformation provided by API-Kolon.
Izod Impact, Notched 1.08 J/cm

@Thickness 6.35 mm,
Temperature 22.8 °C
2.02 ft-lb/in

@Thickness 0.250 in,
Temperature 73.0 °F
ASTM D256
Global HI-650 High Impact Polystyrene
High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys
Izod Impact, Notched >= 1.08 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 2.02 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GP2300 PC+GF30%, Heat Resistance
Description: Injection Molding, PC+GF30%, General Purpose, Heat ResistanceApplication: IT/OA, E&E Housing and Components, Automotive (Interior)CAS: 103598-77-2 and 65997-17-3Information provided by ..
Izod Impact, Notched 1.08 J/cm

@Temperature 23.0 °C
2.02 ft-lb/in

@Temperature 73.4 °F
ASTM D256
LG Chemical SEETEC T3410 Polypropylene Random Terpolymer
Features: Seetec T3410 is a polypropylene-ethylene-butene random terpolymer designed for the production of Transparent Film and Expandable PP for low seal temperature and high impact strength. It of..
Izod Impact, Notched >= 1.08 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
>= 2.02 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GN2201FM PC+GF20%, Halogen Free, Flame Retardant, Heat Resistance
Description: Injection Molding, PC+GF20%, Halogen Free Flame Retardant, Heat ResistanceApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2 and 65997-17-3Information prov..
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
Shinil Chemical SHINSTRA PA-6 AG30N Structural Polymer Wheel Cover
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® NH-3402F PC, 40% Glass Filled FR
PC/GF material with 40% GF reinforcement that can be used in printer LSUInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 1.08 J/cm

@Thickness 3.17 mm
2.02 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® SF-0950 MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GFN1740V PPE+PS
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL GFN1740V PPE+PS (Europe-Africa-Middle East)
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Toyobo VYLOPET® EMC307 Injection Molding Polyester Resin, High Cycles
Applications: Coiled bobbinsMouthpiecesFeatures: High cyclesInformation provided by Toyobo.
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
Zylog Hipolyene® 5131 SX-5 Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
Cheng Yu Plastic T889G25 PBT, 25% Glass Fiber
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
E-Polymers TEKAPPO® JF2 Un-Reinforced Heat Resistant Chemical Resistance M-PPO
Modified PPO/PPE: TEKAPPO is a modified PPO/PPE, blending PPO with HIPS in order to improve HDT and processability. It displays various HDT range with halogen-free flammability, impact resistance a..
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
E-Polymers SEPAZ® N5020HI Nanoclay 4%, 30% Glass Fiber Reinforced High Impact Nano Composite Resin
Nanocomposite: SEPAZ Nano PA6 nanocomposites have been prepared successfully in commercial scale through 'in situ' polymerization or melt extrusion. The unique performance properties of nanocomposi..
Izod Impact, Notched 1.08 J/cm
2.02 ft-lb/in
ASTM D256
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
Izod Impact, Notched 1.08 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.02 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant
Description: Injection Molding, PC/ABS+GF20%, Halogen Free Flame Retardant, High StiffnessApplication: E&E (Housing, OA Frame)CAS: 103598-77-2, 9003-56-9, 181028-79-5 and 65997-17-3Information provi..