Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
PolyOne Nymax™ GMF 604 40 UV Black 115 1 X 1 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Nylene® Naxel™ PC506 30% Glass Reinforced Polycarbonate Description: Naxel™ PC506 is a 30% glass fiber reinforced polycarbonate. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resourc.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR15 MF25 Glass/Mineral Filled Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Ravago Manufacturing Americas Echo® RPC40G BK Polypropylene Homopolymer Available in North America Filler: Glass Fiber Reinforcement, 40% Filler by weight Recycled Content: YesFeatures: Homopolymer Color: Black Form: Pellets Information provided by Ravago |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Polymer Resources TP-FRG30 Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Polybutylene Terephthalate, 30% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1240MHL BK Nylon 6/6 Available in North America Filler: Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat StabilizedRoHS CompliantForm: Pellets Processing .. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
PolyOne Nymax™ GF 1880 33 HS NATURAL Nylon 6/12, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedHeat StabilizedMolded Test Bars: (Dry as molded:Information provided by PolyOne Corporation. |
|||
Flexural Modulus | 7.21 GPa | 1050 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP EX07305 PEI (Asia Pacific) Polyetherimide reinforced with Glass fiber and PTFE for use in Burn-in Test Sockets (BiTS) Application |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES Electrablend® PA12 CF13 L 13% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 13% Filler by WeightAdditive: LubricantFeatures: Electrically Conductive and lubricatedInformation provided by TP Composi.. |
|||
Flexural Modulus | 7.23 GPa | 1050 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem LTX921A PEI Blend Post-industrial recycle based, 20% glass fiber filled, high flow Polyetherimide blend. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES Electrafil® J-3/CF/10 Nylon 6, 10% Carbon Fiber Reinforced |
|||
Flexural Modulus | 7.26 GPa | 1050 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East) High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear.. |
|||
Flexural Modulus | 7.27 GPa | 1050 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK2000 PC+ABS LNP* Thermocomp* Lexan_JK2000 compound is a 22% GR, ECO-compliant FR, PC+ABS for thinwall molding applications. |
|||
Flexural Modulus | 7.26 GPa | 1050 ksi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Modulus | 7.23 GPa | 1050 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RF005 PA 66 (Asia Pacific) LNP* Thermocomp* RF005 is a compound based on Nylon 66 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 7.25 GPa | 1050 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA6.10 LNP THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Modulus | 7.22 GPa | 1050 ksi | ISO 178 |
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, DRY Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go.. |
|||
Flexural Modulus | 7.22 GPa | 1050 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PX92248 PA 6 LNP* THERMOCOMP* PX92248 is a compound based on Nylon 6 resin containing Proprietary Filler(s). |
|||
Flexural Modulus | 7.25 GPa | 1050 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF QX01581H PA 6/10 (Asia Pacific) LNP* THERMOTUF* QX01581H is a compound based on Nylon 6/10 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Clariant Renol PA2SP0007HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp MF0069S PP LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi.. |
|||
Flexural Modulus | 7.24 GPa | 1050 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightUL File Number: E157318TPCI# 9085101Information provided by TP Composites, Inc. |