PRODUCT NO. Manufacturer Trade Name
Nylene® Norpex® AX30GF , 30% Glass Reinforced Polyphenylene Ether Nylene® Norpex®
Polymer Resources PPX-FRG30 Modified-PPO, V-1 Flame Retardant, 30% Glass Reinforced Polymer Resources, LTD
Polymer Resources PPX-G30 Modified-PPO, 30% Glass Reinforced Polymer Resources, LTD
Polymer Resources PPX-FRG30 Modified PPO, UL 94 V-1, 30% Glass Reinforced  (Unverified Data**)
RTP Company RTP 1701 MG 20  Modified Polyphenylene Oxide (PPO) Glass Fiber 10% - Milled Glass 20% &am
PTS BLACK PPE/Nylon Alloy 30% Glass Filled Polymer Technology & Services, LLC (PTS)
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE LG Chemical LUMILOY
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced LATI Laril
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant LATI Laril
Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled Samsung, Cheil Industries Infino®
Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled
Westlake Plastics Norylux™ Modified Polyphenylene Oxide 30% glass filled Westlake Plastics Norylux™
RTP Company RTP 1705 FR Modified Polyphenylene Oxide (PPO), Glass Fiber - Flame Retardant - Halogen Free RTP Company
Evonik Corporation Vestoran® 1900-GF30 sw PPE Evonik Corporation Vestoran®
E-Polymers TEKAPPO® J930 30% Glass Fiber Reinforced M-PPO E-Polymers Co. Ltd. TEKAPPO®
E-Polymers TEKAMID® JN930 PPE+PA66 30% Glass Fiber Reinforced PA/PPE Alloy E-Polymers Co. Ltd. TEKAMID®
CENTROPLAST CENTROPHEN GF Polyphenylene ether 30% glass fiber CENTROPLAST Engineering Plastics GMBH CENTROPHEN
Ashley Polymers Ashlene® 266 PPO, 30% Glass Reinforced Ashley Polymers Ashlene®
Ashley Polymers Ashlene® P266 PPO, 30% Glass Reinforced Ashley Polymers Ashlene®
Evonik Corporation Vestoran® 1300-GF30 nf PPE Evonik Corporation Vestoran®
Overview of materials for Polyphenylene Ether, 30% Glass Filled
PolyOne Edgetek® MP-30GF/000 Modified PPO - 30% Glass Fiber Reinforced  (discontinued **)
LATI LARIL 13 G/30 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy  (Unverified Data**)&l
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced  (Unverified Data**)
Custom Resins Norpex® GF3 PPE (Polyphenylene Ether), 30% Glass Filled  (discontinued **)
RTP Company RTP 1705  Modified Polyphenylene Oxide (PPO) Glass Fiber 30%  (discontinued **)&
GEHR Plastics PPE-30GF Polyphenylene Ether, 30% Glass Fiber  (discontinued **)
GEHR Plastics Noryl PPO-30 GF 30% Glass Filled  (discontinued **)
LATI LARIL 13 G/30-V1 30% Glass Fiber Reinforced Polyphenylene Oxide (PPOm) (UL94V-1)  (Unverified Data**)
RTP Company RTP 1705 Z  Modified Polyphenylene Oxide (PPO) Glass Fiber 30%  (discontinued **