Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Tygon® Tygoprene® XL-60 Pump Tubing Formulation

Category Polymer , Thermoplastic
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Tygon®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Tygon® Tygoprene® XL-60 Pump Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designed specifically for use in peristaltic pump applications, Tygoprene® Pump Tubing maintains a pump life of over 500 hours. It is extremely flexible and exhibits superior flex life, reducing downtime due to pump tubing failure. Tygoprene® Pump Tubing is translucent in color and has excellent chemical resistance to a wide range of fluids, including acids and bases. It can be considered an alternative to silicones and PVC when longer pump life is required. Features and Benefits Long flex life in peristaltic pumps Low extractables Alternative to PVC Temperature resistant up to 250°F Meets FDA and NSF 51 criteria. Unless otherwise noted, all tests were conducted at room temperature. Values shown were determined on 1.9 mm thick extruded strip or 1.9 mm thick molded ASTM plaques or molded ASTM durometer buttons.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792-00
Water Absorption 0.070 %

@Temperature 22.8 °C,
Time 86400 sec
0.070 %

@Temperature 73.0 °F,
Time 24.0 hour
ASTM D570-98
Mechanical Properties Metric English Comments
Hardness, Shore A 60

@Time 15.0 sec
60

@Time 0.00417 hour
ASTM D2240-03
Tensile Strength 11.2 MPa
1630 psi
ASTM D412-98
Elongation at Break 770 %
770 %
ASTM D412-98
100% Modulus 0.00383 GPa
0.555 ksi
ASTM D412-98
Tear Strength 33.3 kN/m
190 pli
ASTM D1004-03
Compression Set 55 %

@Temperature 70.0 °C,
Time 79200 sec
55 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395-03 Method B
Tensile Set 100 %
100 %
ASTM D412-98
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Brittleness Temperature -66.1 °C
-87.0 °F
ASTM D746-98
Electrical Properties Metric English Comments
Dielectric Strength 21.7 kV/mm
550 kV/in
ASTM D149-97
Compliance Properties Metric English Comments
FDA Yes
Yes
NSF Yes
Yes
Descriptive Properties Value Comments
Color Translucent
Copyright © lookpolymers.com All Rights Reserved