Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -66.1 °C | -87.0 °F | ASTM D 746 |
CPT C-Flex® R70-046 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Brittleness Temperature | -66.1 °C | -87.0 °F | ASTM D 746 |
CPT C-Flex® R70-050 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Brittleness Temperature | -66.1 °C | -87.0 °F | ASTM D746-98 |
Saint-Gobain Tygon® Tygoprene® XL-60 Pump Tubing Formulation Designed specifically for use in peristaltic pump applications, Tygoprene® Pump Tubing maintains a pump life of over 500 hours. It is extremely flexible and exhibits superior flex life, reducing do.. |