Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SPS Guang Zhou POLLITEâ„¢ 1002G30 Flame-retarded/GF30%-Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Glass Fiber Filled, Flame Retardant
Manufacturer SPS Guang Zhou
Trade Name POLLITE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPS Guang Zhou POLLITEâ„¢ 1002G30 Flame-retarded/GF30%-Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristic: High mechanical properties, high rigidity, high heat resistant, good dimensional stability, good flame retardanceApplications: E/E parts, power tool, office suppliesInformation Provided by SPS (Guang Zhou) Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D792
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 120 MPa
17400 psi
ASTM D638
Flexural Strength 155 MPa
22500 psi
Flexural Modulus 6.70 GPa
972 ksi
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 152 °C
306 °F
ASTM D648
Flammability, UL94 V-0
V-0