Material Notes:
Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel
Physical Properties Metric English Comments
Volatiles 1.0 - 4.0 %
1.0 - 4.0 %
Prepreg
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.0097-0.011
Laminate
Dry Resin Content (%) 36-40
Prepreg
Fiber Volume (%) 50-55
Laminate
Flow (%) 13-25