Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CM4219 PC+ABS (Asia Pacific) |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX9136C PC COPOLYMER (Europe-Africa-Middle East) Lexan* LUX9136C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry As Molded
&nbs AMODEL AFA-6133 V0 is a 33% glass-fiber reinforced grade of polyphthalamide (PPA) resin that was developed specifically for connector applications requiring compatibility with both "infrared" and "v.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX9130C PC COPOLYMER (Asia Pacific) Lexan* LUX9130C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4 is a 40% fiberglass reinforced polyphenylene sulfide compound which provides outstanding chemical resistance and mechanical properties even at.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp ICP36 PA 6/12 (Asia Pacific) LNP* Lubricomp* ICP36 is a compound based on Nylon 6/12 resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, , Electrically Conductive.This data was .. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WFL34H PBT (Asia Pacific) LNP* LUBRICOMP* WFL34H is a compound based on Polybutylene Terephalate resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry) Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1125 HS Polyphthalamide (PPA), 25% Glass Fiber (Conditioned) Amodel® AT-1125 HS polyphthalamide (PPA) is a toughened, heat stabilized 25% glass reinforced resin, designed as a cost effective solution for applications requiring stiffness, good dimensional s.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem CRS5211 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Thi.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 420R PBT (Asia Pacific) 30% GR, ex strength/stiffness/dimensional stability; heat resistance. Appliance handles, spotlights, electric motors, etc. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacif.. |
|||
Izod Impact, Notched | 0.850 J/cm @Thickness 3.18 mm |
1.59 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 553 PBT+PC (Asia Pacific) 30% GR PBT+PC, UL94 V-0. Reduced warpage characteristics.Applications; appliance handles, spotlights, electric motors, pump housings, etc. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQ8280SF PBT+PET Valox iQ8280SF resin is an environmentally responsible, low carbon footprint, and sustainable resin. Valox iQ8280SF resin offer Super High Flow characteristics combined with high modulus and excell.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF00469S PA 66 LNP* THERMOCOMP* RF00469S is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp RF0049S PA 66 LNP THERMOCOMP* RF0049S is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP fo.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp RF0049S PA 66 (Asia Pacific) LNP THERMOCOMP* RF0049S is a compound based on Nylon 66 resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP fo.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing 30% Glass Fiber. Added features include: Healthcare. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EF006H PEI (Asia Pacific) LNP* Thermocomp* EF006H is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP UF006S PPA (Asia Pacific) LNP THERMOCOMP* UF006S is a compound based on Polyphthalamide resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL FXN4020H PPE+HIPS (Asia Pacific) high gloss Noryl |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PV300G2 ABS, 10% Glass Fiber 10% glass fiber reinforced ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 67MG Nylon 66, Glass/Mineral reinforced A glass/mineral reinforced Nylon 66 designed for high strength and dimensional stability.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.850 J/cm | 1.59 ft-lb/in | ASTM D256 |
Chevron Phillips Xtel® XK2040 Polyphenylene Sulfide Alloy
(discontinued **) Natural Color Polyphenylene Sulfide AlloyXtel™ XK2040 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties alo.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature -30.0 °C |
1.59 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® LUX7632C PC COPOLYMER (Asia Pacific) Lexan* LUX7632C Polycarbonate (PC) resin is a non-filled, extrudable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is U.. |
|||
Izod Impact, Notched | 0.850 J/cm @Temperature 23.0 °C |
1.59 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamTal PM3007G6 Acetal, 30% Glass Fiber 30% Glass-fiber reinforced polyacetal for injection molding applications.Information provided by Polyram Ram On Ind. |