Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend (Europe-Africa-Middle East) High heat amorphous TPI Blend, Chemical Resistant |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics EXTEM UH1016 TPI Blend (Asia Pacific) High heat amorphous TPI Blend, Chemical Resistant, High Flow |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Grupo Repol Dinalon® B1S25 G30PV0 30% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 6 Mechanical properties are for dry as molded samples.Information provided by Grupo Repol. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East) VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 5031 PBT (Europe-Africa-Middle East) VALOX 5031 is a 30% glass reinforced PBT+PC blend with low warpage characteristics. Applications: appliance handles, automotive doorhandles. This grade is a 508 with reduced warpage. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | SABIC - Japan Method |
SABIC Innovative Plastics Valox® 553M PBT+PC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 120 MPa @Strain 0.200 %, Temperature 425 °C |
17400 psi @Strain 0.200 %, Temperature 797 °F |
Precipitation Hardened prior to test |
Special Metals INCOLOY® Alloy DS A nickel-iron-chromium alloy with an addition of silicon. It has good high-temperature strength and excellent resistance to oxidation and carburization. The silicon content makes the alloy resista.. |
|||
Tensile Strength, Yield | 120 MPa @Temperature 300 °C |
17400 psi @Temperature 572 °F |
Annealed prior to test |
Special Metals Nickel 200 Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
SPS Guang Zhou POLLITEâ„¢ 1002G30 Flame-retarded/GF30%-Polycarbonate Characteristic: High mechanical properties, high rigidity, high heat resistant, good dimensional stability, good flame retardanceApplications: E/E parts, power tool, office suppliesInformation Provi.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WF007 PBT LNP THERMOCOMP WF007 is a compound based on PBT resin containing 35% Glass Fiber. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® HX420HP PBT (Europe-Africa-Middle East) Medium Flow, 30% Glass filled, Polybutylene Terephthalate (PBT) resin. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
Tipco Tipcofil® AG 300 - 15% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 15% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM-D638 |
Polyram PlusTek RA325G5 Nylon 6.6, 25% Glass Fiber, Flame Retardant 25% glass fiber reinforced, self extinguishing halogen free polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Polyram Polytron P40B07 Polypropylene, 40% Long Glass Fiber, UV Stabilized A chemically coupled 40% long glass fiber reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM-D638 |
Polyram Polytron P50B03 Copolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteristi.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Polyram Polytron P40N11 Polypropylene, 40% Long Glass Fibers A chemically coupled 40% long glass fiber reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Eurostar Staramide RF004XXC PA6, 20% Glass Fiber Filled, Injection Molded Staramide RF004XXC is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | v = 50 mm/min; ISO 527-2 |
CENTROPLAST CENTROMID 6 GF 30 Polyamide 6 30% glass fiber The 30% glass fibre matrix adds very high strength and rigidity to this material. It has increased dimensional accuracy when hot. Can be used for rollers, belt pulleys and racks.Information provid.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ASTM D638 |
Beijing Ranger Chem PBT-201-G30 211 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527-2 |
Ascend Performance Materials Vydyne® R860 BK02 Nylon 66, Glass/Mineral Reinforced, DAM Vydyne® R860 BK02 is general-purpose, glass-fiber and mineral-reinforced PA66 resin. Available in black, this product is also lubricated for improved flow and offers superior surface appearance. Gl.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 50mm/min; ISO 527 |
BASF Ultramid® A3WG5 25% Glass Filled PA66 (Conditioned) Ultramid A3WG5 is a 25% glass fiber reinforced and heat resistance injection molding PA66 grade. |
|||
Tensile Strength, Yield | 120 - 220 MPa | 17400 - 31900 psi | |
ArcelorMittal 54+AS Aluminized steel Use: Difficult drawingInformation provided by ArcelorMittal |
|||
Tensile Strength, Yield | 120 - 180 MPa | 17400 - 26100 psi | |
ArcelorMittal 56+AS Aluminized steel Use: Extra-deep drawingInformation provided by ArcelorMittal |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 50 mm/min; ISO 527-2 |
BASF Ultradur® S 4090 G6 High Speed 30% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 30% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | 50 mm/min; ISO 527-2 |
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET PBT + PET, injection-molding grade containing 20% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor housin.. |
|||
Tensile Strength, Yield | 120 MPa | 17400 psi | ISO 527 |
Polyram RamSter PF321G4 PBT, 20% Glass Fiber, Flame Retardant 20% Glass fiber reinforce, flame retardant PBT for injection molding applications.Information provided by Polyram. |