Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO-15 PP, Flame Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer S&E Specialty Polymers
Trade Name TufGuard M™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO-15 PP, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers
Physical Properties Metric English Comments
Specific Gravity 0.980 - 1.02 g/cc
0.980 - 1.02 g/cc
ASTM D792
Melt Flow 13.0 - 17.0 g/10 min
13.0 - 17.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 22.8 MPa
>= 3300 psi
ASTM D638
Elongation at Break >= 60.0 %
>= 60.0 %
Ultimate; ASTM D638
Flexural Modulus 1.21 GPa
175 ksi
tangent; ASTM D790
Izod Impact, Notched >= 1.60 J/cm
>= 3.00 ft-lb/in
ASTM D256
Falling Dart Impact >= 20.3 J
>= 15.0 ft-lb
ASTM D5420
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 3.17 mm
V-0

@Thickness 0.125 in
Oxygen Index >= 28.0 %
>= 28.0 %
ASTM D2863
Copyright © lookpolymers.com All Rights Reserved