Material Notes:
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a wide service range from -20 degrees C to 120 degrees C, high tear resistance, low density, and good paintability.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D792
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 8.0 g/10 min
8.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
ASTM D2240
Tensile Strength, Ultimate 8.30 MPa
1200 psi
ASTM D638
Flexural Modulus 0.200 GPa
29.0 ksi
ASTM D790
Tear Strength 63.1 kN/m
360 pli
ASTM D624