Physical Properties Metric English Comments
Melt Flow 13.0 g/10 min
13.0 g/10 min
ASTM D1238
S&E Specialty Polymers TufFill NH™ 2102A PP, Flame Retardant
Application: A polypropylene based, zero halogen, flame retardant compound with antistatic properties designed for packaging applications.Information provided by S&E Specialty Polymers
Melt Flow 13.0 - 17.0 g/10 min
13.0 - 17.0 g/10 min
ASTM D1238
S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO PP, Flame Retardant
Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers
Melt Flow 13.0 - 17.0 g/10 min
13.0 - 17.0 g/10 min
ASTM D1238
S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO-15 PP, Flame Retardant
Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers
Melt Flow 13.0 - 18.0 g/10 min
13.0 - 18.0 g/10 min
ASTM D1238
S&E Specialty Polymers TufGuard M™ GPP1005M-CD PP, Flame Retardant
Application: A UL94 V-2, flame retardant polypropylene compound for injection molding applications, including cases for industrial power supply. Compound is designed with halogen-based flame retarda..
Melt Flow 13.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
13.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP 7002 Thermoplastic Elastomer
Notes: Semi-transparent Features: Good Chemical and Oil ResistanceInformation Provided by Teknor Apex
Melt Flow 13.0 g/10 min

@Load 2.16 kg,
Temperature 125 °C
13.0 g/10 min

@Load 4.76 lb,
Temperature 257 °F
ASTM D1238
Teknor Apex Monprene® MP-1900-R Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 13.0 g/10 min

@Load 5.00 kg,
Temperature 235 °C
13.0 g/10 min

@Load 11.0 lb,
Temperature 455 °F
ASTM D1238
Teknor Apex Chemlon® 282 Nylon 6, Non-halogenated
Features: Flame Retardant; General Purpose; Halogen-free; U.L. 94 V-O at 0.63 mm; ColorableProcessing Method: Injection Molding Forms: Pellets Additive: Flame RetardantInformation Provided by Teknor..
Melt Flow 13.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
13.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1426A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 13.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
13.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2815A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 13.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Synres® SR 4336 Polypropylene
Notes: The Specialty Compounding Division offers a proprietary line of mineral filled polyolefins, including talc and calcium carbonate filled polypropylenes. Typical applications include injection ..
Melt Flow 13.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4955F Thermoplastic Elastomer
Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T..
Melt Flow 13.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL 83-F943D22-NT Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 13.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
13.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1182A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 13.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
13.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Telcar® TL-1934A Styrenic Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Flexible Cord Jacketing; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581Forms: P..
Melt Flow 13.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
13.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron IM14GL ABS Injection Molding Grade
Super High Rigidity, Medium Impact, High Chemical ResistanceInformation provided by Bhansali
Melt Flow 13.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
13.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron SE32H Extrusion ABS
Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali
Melt Flow 13.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
13.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron SE32H Extrusion ABS
Very High Impact, Better Flow and Sheet/Pipe/Profile applicationInformation provided by Bhansali
Melt Flow 13.0 g/10 min

@Load 10.0 kg,
Temperature 220 °C
13.0 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238