Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D638 |
S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO PP, Flame Retardant Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-0212 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2 in per min; ASTM D638 |
Network Polymers NPP 25-2003 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 22.8 MPa @Thickness 3.20 mm |
3300 psi @Thickness 0.126 in |
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 2150 H Medium Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2" (50mm) per min.; ASTM D638 |
Formosa Plastics Formolene® L63935U Rotational Molding LLDPE
(discontinued **) Hexene CopolymerApplications: Tanks, toys and other non-tank rotational molding applicationsFormolene L63935U is fully heat and UV stabilized.Meets all requirements of the U.S. Food and Drug Adminis.. |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total Finathene® 3407B Black HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 51 mm/min; ASTM D638 |
I. Stern 320NB Prime Impact Copolymer Polypropylene, No Break Features:Outstanding impact strength balanced with stiffnessExcellent long term heat aging propertiesWet/dry environment resistanceGood surface glossApplicationsAutomotiveApplianceLawn and GardenRig.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 51 mm/min; ASTM D638 |
I. Stern 3320 Prime Impact Copolymer Polypropylene Features:Excellent balance of stiffness and impact strengthExcellent long term aging propertiesExcellent color and process stabilityApplicationsClosuresHousewaresSmall appliancesLawn and GardenInfor.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
Global HI-650 High Impact Polystyrene High flowGood stiffnessApplications:AppliancesElectrical/Electronic applicationsHousehold goodsFood packagingToys |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2 in/min; ASTM D638 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. .. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
Multibase Multi-Flamâ„¢ 0901 HDPE Polyethylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Blow MoldingExtrusionCoextrusionUses:TubingFurniturePipingInformation provided by Multibase |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | Compound; ASTM D638 |
Borealis Borcell™ HE1344 High Density Polyethylene Compound for Cellular Insulation of Data Cables Borcell HE1344 is a high-molecular weight, high-density polyethylene (HDPE) insulation compound containing an industry approved non plate-out chemical blowing agent. It contains the required levels.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2"/min; ASTM D638 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2"/min; ASTM D638 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total CD 4300 HDPE extrusion Applications: General profile extrusion, irradiation-crosslinked productsInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene Impact Copolymer for High Speed injection Molded Applications Formolene® 6575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging,.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2"/min; ASTM D638 |
A. Schulman LP390-01 Narrow Molecular Weight Copolymer DescriptionLP 390-01 natural is a narrow molecular weight copolymer, high density polyethylene combining excellent impact strength with good environmental stress crack resistance.ApplicationLP 390-0.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
A. Schulman POLYFORT™ FPP 2067HU UV Stabilized, High Heat Resistant Impact Polypropylene DescriptionPolyfort® FPP 2067HU is a unique high flow, UV stabilized high heat resistant impact polypropylene available in matched automotive colors. It molds to a fine appearance with good scrat.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
ExxonMobil HDPE BU46-060 High Density Polyethylene Resin Product Description: BU46-060 is a high molecular weight, high density polyethylene copolymer which contains a UV inhibitor. It possesses a combination of excellent processability, outstanding melt .. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ISO 527-2/1A/50 |
ExxonMobil HDPE HMA 016 High Density Polyethylene Resin Product Description: HMA 016 is a HDPE grade, characterized by fast cycling and good impact strength. It has high gloss and high dimensional stability.Availability: Africa & Middle East, Asia Pacifi.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | Molded and tested per ASTM D4976; ASTM D638 |
Dow UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE) Good extrudability/processability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This produ.. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-638 |
Axiall 1901 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-638 |
Axiall 21540 Coax & Telecom Flexible PVC Black 307 Semi-rigid flame retardant insulation compound with good electrical properties for minimum transmission interference. Suitable for use in riser insulation. Max service temperature rating of 80°C .. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPS 100-3 HIPS Black Extrusion Grade Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinFeatures: A high impact Polystyrene, custom colored black, featuring good flow and excellent toughness for all extrusion applications. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D638 |
Asahi Kasei Thermofil P-40CC-1100 40% Calcium Carbonate Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | ASTM D-638 |
Axiall 21570 Coax & Telecom Flexible PVC Semi-rigid insulation compound designed for data communication riser cable applications. Maximum 75°C service temperature rating.Information provided by Georgia GulfGeorgia Gulf became Axiall Corp.. |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total Finathene® 4344 HDPE, blow molding
(discontinued **) Applications: storage tank liners, intermediate bulk containers, general large-part blow molding. Blow Molding Stock Temperature 370 – 410 ºFInformation provided provided by Total Petrochemicals.T.. |
|||
Tensile Strength, Yield | >= 22.8 MPa | >= 3300 psi | ASTM D 638 type IV |
Total CD 471 HDPE conduit Applications: Wire and cable conduit, fiber optic innerductInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines. |
|||
Tensile Strength, Yield | 22.8 MPa | 3300 psi | 2 in/min; ASTM D638 |
Ineos H48-500-199 Polyethylene Copolymer This is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for roll-out cart applications. This material meets the Food and Drug Administration req.. |