Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.0 - 17.0 g/10 min | 13.0 - 17.0 g/10 min | ASTM D1238 |
S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO PP, Flame Retardant Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers |
|||
Melt Flow | 13.0 - 17.0 g/10 min | 13.0 - 17.0 g/10 min | ASTM D1238 |
S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO-15 PP, Flame Retardant Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers |
|||
Melt Flow | 5.00 - 17.0 g/10 min | 5.00 - 17.0 g/10 min | Average value: 9.67 g/10 min Grade Count:9 |
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim.. |
|||
Melt Flow | 0.100 - 17.0 g/10 min | 0.100 - 17.0 g/10 min | Average value: 6.10 g/10 min Grade Count:34 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Melt Flow | 3.00 - 17.0 g/10 min | 3.00 - 17.0 g/10 min | Average value: 10.1 g/10 min Grade Count:36 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Melt Flow | 2.00 - 17.0 g/10 min | 2.00 - 17.0 g/10 min | Average value: 9.87 g/10 min Grade Count:19 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |