Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Falling Dart Impact | >= 20.3 J | >= 15.0 ft-lb | ASTM D5420 |
S&E Specialty Polymers TufGuard M™ GPP1001VOM-HCO-15 PP, Flame Retardant Application: UL-94 V0 Flame Retardant/Impact Resistant PolypropyleneInformation provided by S&E Specialty Polymers |
|||
Falling Dart Impact | 20.3 - 47.5 J | 15.0 - 35.0 ft-lb | Average value: 34.3 J Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Sheet". Each property range of values reported is minimum and max.. |
|||
Falling Dart Impact | 20.3 J @Temperature -40.0 °C |
15.0 ft-lb @Temperature -40.0 °F |
ASTM D3029 |
Spartech Centrex SP-6710 Weatherable Sheet Description: Weatherable SheetCentrex is a registered trademark of Bayer Corporation.Information provided by Spartech. |
|||
Falling Dart Impact | 20.3 J | 15.0 ft-lb | 73°F; ASTM D3029 |
Spartech SP-9030 Economy ABS Sheet Description: ABS SheetInformation provided by Spartech. |
|||
Falling Dart Impact | 20.3 J | 15.0 ft-lb | 73°F; ASTM D3029 |
Spartech SP-9080 High Heat ABS Sheet Description: ABS SheetInformation provided by Spartech. |