Material Notes:
Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsRecommended Applications:Automotive, motorcycle and electrical appliance parts that require excellent flowability such as washing tube and tubInformation provided by SCG Chemicals
Physical Properties Metric English Comments
Specific Gravity 0.910 g/cc
0.910 g/cc
ASTM D1505
Linear Mold Shrinkage, Flow 0.0142 cm/cm

@Thickness 2.00 mm
0.0142 in/in

@Thickness 0.0787 in
TPE Method
Linear Mold Shrinkage, Transverse 0.014 cm/cm

@Thickness 2.00 mm
0.014 in/in

@Thickness 0.0787 in
TPE Method
Melt Flow 43 g/10 min

@Load 2.16 kg,
Temperature 230 °C
43 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength at Break 18.0 MPa
2610 psi
ASTM D638
Tensile Strength, Yield 28.4 MPa
4120 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm

@Temperature -20.0 °C
0.551 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.392 J/cm

@Temperature 0.000 °C
0.735 ft-lb/in

@Temperature 32.0 °F
ASTM D256
0.686 J/cm

@Temperature 23.0 °C
1.29 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 163 °C
325 °F
ASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525
Brittleness Temperature -20.0 °C
-4.00 °F
ASTM D746
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Haze 80 %

@Thickness 1.00 mm
80 %

@Thickness 0.0394 in
ASTM D1003
Gloss 30 %

@Thickness 1.00 mm
30 %

@Thickness 0.0394 in
ASTM D2457