Material Notes:
Description: Polyacid dispersant. Highly versatile, economical and low foam, flat to gloss, ideal for interior application.Identification: ACRYLIC POLYMERCAS: 9003-04-7Available in: North America IR Spectrum: 0.31-0.61, RP-17642Applications: RHODOLINE© 270 is a highly efficient anionic dispersant for pigments used in latex paints and adhesives. Use RHODOLINE© 270 at 0.6 – 1.0% (dry basis) by weight on pigment, depending upon the system. The optimum use level of RHODOLINE© 270 may be determined by the pigment dispersant demand method.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.30 - 1.33 g/cc
0.0470 - 0.0480 lb/in³
RP-17617
Solids Content 42.8 - 43.3 %

@Temperature 130 °C,
Time 1800 sec
42.8 - 43.3 %

@Temperature 266 °F,
Time 0.500 hour
0.5 g; RP-0540
pH 7.0 - 8.0
7.0 - 8.0
RP-0420
Viscosity 100 - 300 cP
100 - 300 cP
#2 sp @ 30 rpm; RP-0596
Molecular Weight 3400 g/mol
3400 g/mol
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear, Colorless to yellow liquid
RP-0064