Mechanical Properties Metric English Comments
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
PolyMirae Moplen EP300K Injection Molding Grade Polypropylene
Moplen EP300K is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300K is a block copolymer particularly suitable for injection..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
PolyMirae Moplen HP310R Extrusion Coating and Lamination Grade Polypropylene
Moplen HP310R is the polypropylene copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP310R is a copolymer particularly suitable for extrusion coating and..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
PolyMirae Moplen RP340N Injection Molding Grade Polypropylene
Moplen RP340N is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340N is a random copolymer particularly suitable for injecti..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
PolyMirae Moplen RP344R Injection Molding Grade Polypropylene
Moplen RP344R is a nucleated polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP344R is a random copolymer particularly suitable for..
Flexural Modulus 1.23 GPa
179 ksi
Tangent; ASTM D790
Multibase Nylex™ 2185 FR Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodFlame RetardantForms:PelletsProcessing Methods:Injection MoldingUses: Electric..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
PolyMirae Moplen EP401M Injection Molding Grade Polypropylene
Moplen EP401M is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP401M is a block copolymer particularly suitable for injection..
Flexural Modulus 1.23 GPa
179 ksi
1% Secant; 12.5 mm/min; ASTM D790
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade  (discontinued **)
ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
LyondellBasell Alathon® L5440 High Density Polyethylene
ApplicationsALATHON L 5440 is designed for high shear machines. It exhibits excellent color, low odor and excellent processing stability. Typical applications include general purpose, household ch..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
Hyosung Topilene J640A PP
J640A Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporatio..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790A
Ineos H03G-05 Polypropylene Homopolymer
Grade H03G-05 is a polypropylene homopolymer designed for BOPP applications and meet the requirements of the U.S. Food and Drug administration as specified in 12 CFR 177.1520.Applications:Food Packa..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D760
LG Chemical SEETEC M1500 Polypropylene Impact Copolymer
SEETEC M1500 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1500 exhibits a high flowability and a good balance of stiffness and impact strength. SEETEC M1500 ..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D760
LG Chemical SEETEC M1600 Polypropylene Impact Copolymer
Features: SEETEC M1600 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1600 exhibits a high flowability and a good balance of stiffness and impact strength. SEE..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D760
LG Chemical SEETEC M1700 Polypropylene Impact Copolymer
Features: SEETEC M1700 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1700 exhibits a very high flowability and a good balance of stiffness and impact strength..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H5814J High Density Polyethylene Injection Molding
Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding
Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P840J Polypropylene Injection Molding
Key Characteristics:Excellent flowabilityExcellent processabilityHigh stiffnessSuitable for complex parts and large partsRecommended Applications:Automotive, motorcycle and electrical appliance part..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P851JO Polypropylene Injection Molding
Key Characteristics:Good processabilityHigh gloss and brightnessOdorlessSafe for food contactRecommended Applications:Clear food containerClear large size containerThin wall productsInformation prov..
Flexural Modulus 1.23 GPa
178 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P852J Polypropylene Injection Molding
Key Characteristics:Excellent productivityHigh clarityHigh stiffnessRecommended Applications:Clear food containerClear large size containerHousehold products and other articles that require high tra..
Flexural Modulus 1.23 GPa
178 ksi
Zylog Hipolyene® 2530 DW Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.
Flexural Modulus 1.23 GPa
178 ksi
Zylog Hipolyene® 4955 T Thermoplastic Polyolefin & PP Compound
Information provided by Zylog Plastalloys Pvt. Ltd.