SABIC Innovative Plastics SABIC STAMAX 40YM243 PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name SABIC STAMAX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics SABIC STAMAX 40YM243 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SABIC® STAMAX 40YM243 is a 40% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 209768490.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Filler Content 40 %
40 %
glass; ISO 3451
Mechanical Properties Metric English Comments
Tensile Strength at Break 108 MPa
15700 psi
Type I, 50 mm/min; ASTM D638
121 MPa
17500 psi
50 mm/min, 1A; ISO 527
54.0 MPa

@Temperature 120 °C
7830 psi

@Temperature 248 °F
50 mm/min, 1A; ISO 527
75.0 MPa

@Temperature 80.0 °C
10900 psi

@Temperature 176 °F
50 mm/min, 1A; ISO 527
Elongation at Break 1.8 %
1.8 %
Type I, 50 mm/min; ASTM D638
2.1 %
2.1 %
50 mm/min; ISO 527
Tensile Modulus 8.30 GPa
1200 ksi
1 mm/min; ISO 527
8.47 GPa
1230 ksi
50 mm/min; ASTM D638
4.50 GPa

@Temperature 120 °C
653 ksi

@Temperature 248 °F
1 mm/min; ISO 527
5.70 GPa

@Temperature 80.0 °C
827 ksi

@Temperature 176 °F
1 mm/min; ISO 527
Flexural Modulus 7.67 GPa
1110 ksi
1.3 mm/min, 50 mm span; ASTM D790
7.85 GPa
1140 ksi
2 mm/min, 64mm span; ISO 178
5.55 GPa

@Temperature 80.0 °C
805 ksi

@Temperature 176 °F
2 mm/min, 64mm span; ISO 178
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4mm, Cut; ISO 180/1A
Charpy Impact, Notched 2.20 J/cm²
10.5 ft-lb/in²
80*10*4mm, Cut; ISO 179/1eA
2.80 J/cm²

@Temperature -30.0 °C
13.3 ft-lb/in²

@Temperature -22.0 °F
80*10*4mm, Cut; ISO 179/1eA
Dart Drop, Total Energy 8.00 J

@Temperature 23.0 °C
5.90 ft-lb

@Temperature 73.4 °F
Instrumented Impact Energy @ peak, 6.6 m/s; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 157 °C
315 °F
80*10*4mm, Cut; ISO 75-1&2
158 °C

@Thickness 3.20 mm
316 °F

@Thickness 0.126 in
ASTM D648