Polymer Property : Izod Impact, Notched (ISO) = 8.09 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics GELOY HRA222F ASA+PC
Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application..
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRICOMP DFL36ELH PC
LNP* Lubricomp* DFL36ELH is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractible, Easy Moldi..
Izod Impact, Notched (ISO) 17.0 kJ/m²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Total Lacqtene® 2003 PBK 41 HDPE pipe, sheet  (discontinued **)
LACQTENE® 2003 PBK 41 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2003 PBK 41 is a black compound especially developed for i..
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1A
Celanese VECTRA A435 LCP, 35% Specialty  (Unverified Data**)
Good High Current Arc Ignition (HAI) performance. Glass/PTFE filled.Glass/PTFE, good high High Arc Ignition performanceA three-zone screw evenly divided into feed, compression, and metering zones i..
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1A
Celanese VECTRA MT1335 LCP, Medical Technology  (Unverified Data**)
Good High Current Arc Ignition (HAI) performance. Glass/PTFE filled.Glass/PTFE, good high High Arc Ignition performanceA three-zone screw evenly divided into feed, compression, and metering zones i..
Izod Impact, Notched (ISO) 17.0 kJ/m²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 180/1A
Grupo Repol Dinalon® B1S25 G50 50% Glass Fiber Reinforced Nylon 6
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1eA
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc..
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1eA
Solvay TECHNYLSTARâ„¢ AFX 218 V50 PA6, 50% glass filled, DRY
Description TECHNYLSTARâ„¢ AFX 218 V50 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. It is availab..
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4mm, Cut; ISO 180/1A
SABIC Innovative Plastics SABIC STAMAX 40YM240 PP
SABIC® STAMAX 40YM240 is a 40% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 16497161...
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRILOY DF206XXH PC
LNP* LUBRILOY* DF206XXH is a compound based on Polycarbonate containing 30% Glass Fiber, Proprietary Lubricant. Added features of this grade include: Wear Resistant, Healthcare.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP STAT-KON WEF32ISP PBT (Europe-Africa-Middle East)
LNP * Stat-kon* WEF32ISP is a compound based on Polybutylene Terephalate resin containing Glass Fiber and Carbon Fiber. Added features include High Impact, Heat Stabilized and Electrically Conduct..
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 (Asia Pacific)
LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOCOMP TH0815A PUR (Asia Pacific)
LNP* THERMOCOMP* TH0815A is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1A
Styron Magnumâ„¢ 3416 SC Natural Plus ABS Resin
The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent processability with sable light base color that is ideal for self-coloring.Information provided by Do..
Izod Impact, Notched (ISO) 17.0 kJ/m²

@Temperature -40.0 °C
8.09 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural.
Izod Impact, Notched (ISO) 17.0 kJ/m²

@Temperature -40.0 °C
8.09 ft-lb/in²

@Temperature -40.0 °F
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS (Europe-Africa-Middle East)
LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing Long Glass. Added features of this material include: Easy Molding.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East)
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP THERMOTUF VF008 Super Tough Nylon
LNP THERMOTUF* VF008 is a compound based on Super Tough Nylon resin containing Glass Fiber. Added features of this material include: High Impact.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON MVL36SX0 PP (Europe-Africa-Middle East)
LNP* VERTON* MVL36SX0 is a compound based on PP resin containing Long Glass Fiber and PTFE. Added features include: Chemically coupled, Heat Stabilized, Internally Lubricated.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180-93
Wellman Wellamid® XT1606-N Impact Modified Nylon 66
Description: Impact Modified Nylon 66Information provided by Wellman.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180
Polyram RamTough PZ513 Polycarbonate, Easy Flow, Flame Retardant
Transparent polycarbonate, UV stabilized, easy flow, flame retardant, for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
Conditioned; ISO 180/1A
Addiplast Addinyl A2 ZV40 Nylon 66, 40% Glass Filled
Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1A
Celanese VECTRA A435 LCP, 35% Specialty
Best High Current Arc Ignition (HAI) performance. Glass/PTFE filled.Information provided by Celanese
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1A
Celanese VECTRA A725 LCP, 25% Specialty
Conductive Vectra grade, smooth surface compared to A700. 25% filled grade.Information provided by Celanese
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO 180/1A
Celanese VECTRA MT1335 LCP, Medical Technology
Best High Current Arc Ignition (HAI) performance. Glass/PTFE filled.Information provided by Celanese
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
ISO Test
BASF Ultramid® TG3S BK-104 15% Glass Filled PA6 (Dry)
Ultramid TG3S BK-104 is a 15% glass reinforced, heat stabilized, impact modified PA6 injection molding compound developed for applications requiring improved toughness in combination with a balance ..
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP VERTON RX970079 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX970079 is a compound based on PA 66 resin containing Long Glass Fiber and PTFE. Added features include; Internally Lubricated.
Izod Impact, Notched (ISO) 17.0 kJ/m²
8.09 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics NORYL PX2355 PPE+HIPS (Europe-Africa-Middle East)
NORYL PX2355 is an unfilled, medium heat, low odour and low emission material with excellent heat aging performance. It has been developed for automotive interior applications, such as instrument pa..
Izod Impact, Notched (ISO) 17.0 kJ/m²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned)
Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el..