Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.70 GPa | 827 ksi | ASTM D638 |
NCMT NanoPAC™ G2050H High Performance Polypropylene Nanocomposite Applications: Construction MaterialInformation provided by Nano Composite Materials Technology Limited |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1,2 |
Qualchem Danamid FGF-10 Polyamide 6, 10% Glass Fiber Reinforced with glass fiber.Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1,2 |
Qualchem Danamid FGF-15 Polyamide 6, 15% Glass Fiber Reinforced with glass fiber.Information provided by Qualchem Zrt. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | |
Radici Radilon® S ERV3808K (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 5.70 GPa @Temperature 23.0 °C |
827 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B65 G/Mi20 UF grey LS Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP BG004 SAN (Europe-Africa-Middle East) LNP* LUBRICOMP* BG004 is a compound based on Styrene Acrylonitril resin containing Graphite. Added features include: Internally Lubricated. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
Lanxess Durethan® BM 25 FN20 700350 Nylon 6, 25% Mineral PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® DP BKV 240 H2.0 901510 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers reinforced, elastomer-modified, good heat-ageing resistance |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
Lanxess Pocan® BF 4215 000000 PBT, 12% Glass Fiber PBT, 12% glass fibers, injection molding, flame retardant |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 115 000000 Copolyamide, 15% Glass Fiber CoPA, injection molding grade, 15% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 15, even in.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | |
LATI Latilub 87/28-12T G/20 PC, 20% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP MF006SXP PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF006SXP is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Chemically Coupled. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp ZF004XXC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF004XXC is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
Unitika A175G15 PA66, 15% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | cond; ISO 527-1/-2 |
DSM Novamid® 1010GH30 NAT PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Tensile Modulus | 5.70 GPa @Temperature 180 °C |
827 ksi @Temperature 356 °F |
ISO 527-1/-2 |
DSM Stanyl® TE200F8 PA46-GF40 40% Glass Reinforced, Heat Stabilized, for E&E applications |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-3A H PA12-GF30 Grilamid LV-3A H is a 30 % glass fibre reinforced PA12 for injection moulding. Grilamid LV-3A H is very stiff and tough and offers an improved hydrolysis resistance compared to standard PA12 GF 30.I.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30 Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following .. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® CE15315 BK010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK602 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**) 15% Glass Reinforced Polybutylene Terephthalate Crastin SK602 BK851 is a 15% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK261 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 for injection molding. It has excellent surface app.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PFB42ES PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42ES is a Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PFB42EU PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42EU is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam PX05004 PA66, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | |
BASF Procom® GC30S 401 Polypropylene Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-1/-2 |
Lanxess Durethan® BM 25 FN20 DUS013 000000 Nylon 6, 25% Mineral PA 6, injection molding grade, 25% mineral, UL94V-2 off 0.75 mm, max. temp. glow wire test:960°C off 0.8 mm, free from halogen, optimized for laser marking at 1064 nm, |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525H Nylon 66, 25% Glass Filled, Conditioned (2.5% Moisture) Vydyne® R525H is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties whe.. |
|||
Tensile Modulus | 5.70 GPa | 827 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PFB42EU PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB42EU is a compound based on PA 6 resin containing Glass Fiber, Glass Bead. Added features include Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-.. |