Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP VERTON RV007E PA 66 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP VERTON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP VERTON RV007E PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Verton* RV007E is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 214 MPa
31000 psi
5 mm/min; ISO 527
Elongation at Break 2.1 %
2.1 %
5 mm/min; ISO 527
Flexural Strength 309 MPa
44800 psi
2 mm/min; ISO 178
Flexural Modulus 10.2 GPa
1480 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Glow Wire Test 960 °C

@Thickness 0.750 mm
1760 °F

@Thickness 0.0295 in
IEC 60695-2-12
Copyright © lookpolymers.com All Rights Reserved