Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 309 MPa
44800 psi
ISO 178
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA), 33% Glass Fiber
Amodel® AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e..
Flexural Strength 309 MPa
44800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP QC006I PA 6/10
LNP THERMOCOMPâ„¢ QC006I is a compound based on Nylon 6/10 containing 30% Carbon Fiber. Added features of this grade include: High Impact.
Flexural Strength 309 MPa
44800 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP RX00713H PA 66
LNP* Thermocomp* RX00713H is a compound based on Nylon 6/6 containing proprietary fillers. Characteristics of this grade are: Healthcare.
Flexural Strength 309 MPa
44800 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP VERTON RV007E PA 66 (Europe-Africa-Middle East)
LNP* Verton* RV007E is a compound based on Nylon 66 resin containing Long Glass Fiber. Added features of this material include: Easy Molding.
Flexural Strength 309 MPa
44800 psi
ISO 178
SABIC Innovative Plastics LNP VERTON RV007ESS PA 66 (Europe-Africa-Middle East)
LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Flexural Strength 309 MPa
44800 psi
ISO 178
SABIC Innovative Plastics LNP VERTON RX06479 PA 66 (Asia Pacific)
LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Flexural Strength 309 MPa
44800 psi
DAM; ISO 178
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK261 Nylon 6  (Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 6 Zytel PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology only from DuPont it provides exceptional welding resistanceInformation ..
Flexural Strength 309 MPa
44800 psi
ISO 178
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee..
Flexural Strength 309 MPa
44800 psi
ISO 178
SABIC Innovative Plastics LNP VERTON RV007ES PA 66
LNP VERTON* RV007ES is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Flexural Strength 309 MPa
44800 psi
ISO 178
SABIC Innovative Plastics LNP VERTON RX06479 PA 66
LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing 35% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural
Flexural Strength 309 MPa
44800 psi
ISO 178
SABIC Innovative Plastics LNP VERTON RF-7007 EM HS PA 66 (Asia Pacific)
LNP VERTON* RF-7007 EM HS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.