Material Notes:
A general purpose injection molding grade, in black. Also available as: 1043BU (with UV stabilizers).Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
ASTM D570
Moisture Absorption at Equilibrium 0.34 %
0.34 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Melt Flow 10 - 13 g/10 min
10 - 13 g/10 min
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ATSM D638
Elongation at Break 40 %
40 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus 2.00 GPa
290 ksi
ASTM D790
Izod Impact, Notched 6.41 J/cm
12.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 128 °C
262 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 122 °C
252 °F
ASTM D648