Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP ML004S PP (Asia Pacific)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP ML004S PP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* ML004S is a compound based on Polypropylene resin containing PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Time 86400 sec
0.014 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 6.2 %
6.2 %
ASTM D638
Tensile Modulus 1.76 GPa
255 ksi
50 mm/min; ASTM D638
Flexural Strength 41.0 MPa
5950 psi
ASTM D790
Flexural Modulus 1.55 GPa
225 ksi
ASTM D790
Izod Impact, Notched 0.260 J/cm
0.487 ft-lb/in
ASTM D256
Izod Impact, Unnotched 2.79 J/cm
5.23 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C

@Thickness 3.20 mm
144 °F

@Thickness 0.126 in
unannealed; ASTM D648
Users viewing this material also viewed the following: