| Category | Polymer , Thermoplastic , ABS Polymer |
| Manufacturer | Ravago Manufacturing Americas, LLC |
| Trade Name | Hylac® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Ravago Manufacturing Americas Hylac® LG35 Low Gloss ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
| Linear Mold Shrinkage, Flow | 0.0040 - 0.0070 cm/cm <br>@Thickness 3.17 mm |
0.0040 - 0.0070 in/in <br>@Thickness 0.125 in |
ASTM D955 |
| Melt Flow | 3.0 g/10 min <br>@Load 3.80 kg,<br> Temperature 230 °C |
3.0 g/10 min <br>@Load 8.38 lb,<br> Temperature 446 °F |
(Cond. I); ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
| Elongation at Break | 60 % | 60 % | ASTM D638 |
| Tensile Modulus | 1.79 GPa | 260 ksi | ASTM D638 |
| Flexural Yield Strength | 62.7 MPa | 9100 psi | ASTM D790 |
| Flexural Modulus | 2.00 GPa | 290 ksi | ASTM D790 |
| Izod Impact, Notched | 2.67 J/cm <br>@Thickness 3.17 mm |
5.00 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C <br>@Thickness 6.35 mm |
198 °F <br>@Thickness 0.250 in |
unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 78.9 °C <br>@Thickness 6.35 mm |
174 °F <br>@Thickness 0.250 in |
unannealed; ASTM D648 |
| Vicat Softening Point | 106 °C | 223 °F | ASTM 1525 |