Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C @Thickness 3.18 mm |
198 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Maxxam™ PP CS 75 Polypropylene, Unspecified (PP, Unspecified) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C @Thickness 6.35 mm |
198 °F @Thickness 0.250 in |
unannealed; ASTM D648 |
Ravago Manufacturing Americas Hylac® LG35 Low Gloss ABS Acrylonitrile Butadiene Styrene, low gloss ABS.Information provided by Ravago. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | Unannealed; ASTM D648 |
Global PP-2500-H Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-crates, pallets, paint drum, storage & transport container, seatsInformation provided by Global Po.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | Unannealed; ASTM D648 |
Global PP-3240-H Polypropylene Random Copolymer Description-medium stiffness, low melting temperatures, very good for seal Applications-sheets, bottlesInformation provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | ASTM D648 |
Ineos H36G-01 Polypropylene Homopolymer This is a polypropylene homopolymer for general purpose injection molding and high speed fiber spinning applications. It is useful for spunbonded nonwovens and partially oriented yarn (POY). This .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | Unannealed; ASTM D648 |
LyondellBasell Hostacomâ„¢ RTA3184 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | ASTM D648 |
Spartech Weather-Pro G Weatherable Sheet Description: Weatherable SheetInformation provided by Spartech. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS 8003 A1 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Comp.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C @Thickness 3.17 mm |
198 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
Chase Plastics CP Pryme® A300 BK General Purpose (Utility) ABS Molding Resin Information provided by Chase Plastics. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | ISO 75-2/B |
ExxonMobil Exxtral™ BMT222 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by good stiffness/toughness balance and designed for automotive interior applications in which good surface finish and g.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | ISO 75-2/B |
ExxonMobil Exxtral™ LNV 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with high gloss, low warpage, and low discoloration in contact with hot water/steam in large electrical appliance such as washing mach.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0437T30L Talc Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | ASTM D648 |
Americas Styrenics STYRON® 421 High Impact Polystyrene Product CharacteristicsStiffness/FlowHeat resistanceContact clarityFood Contact CompliantUL Classification 94HBTypical ApplicationsAppliancesRefrigerationPackaging/disposablesConsumer electronicsInf.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 92.2 °C | 198 °F | ASTM D648 |
Ineos H20E-00 Polypropylene Homopolymer This is a homopolymer containing antistatic designed for injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Application.. |