Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
Ravago Manufacturing Americas Hylac® LG35 Low Gloss ABS Acrylonitrile Butadiene Styrene, low gloss ABS.Information provided by Ravago. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | at 100%; ASTM D412 |
PB1000-650 Polyurethane-based Biomedical Elastomer |
|||
Tensile Strength, Yield | 36.5 MPa @Thickness 3.17 mm |
5300 psi @Thickness 0.125 in |
ASTM D638 |
PTS Trilac® FR1 ABS- Flame Retardant ABS Resin
(Unverified Data**) Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH034EW Polypropylene, Homopolymer, Slit Film, LWCO COPYLENE™ CH034EW is a medium flow polypropylene homopolymer resin suitable for general injection molding or extrusion applications. Applications: Raffia/tapes/strapping. Equivalent to Pro-fax® HL.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH043EW Polypropylene, Homopolymer, Slit Film, LWCO, Cordage COPYLENE™ CH043EW is a medium flow polypropylene homopolymer resin suitable for general injection molding or extrusion applications. Applications: Raffia/tapes/strapping. Equivalent to Pro-fax® HL.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
M. Holland Company PP700 Polypropylene Homopolymer Features: Antistatic, NucleatedUses: Closure Caps, Thin-walled PartsApprovals: FDA 21 CFR 177.1520Processing Method: Injection MoldingInformation provided by M. Holland. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
Ineos H19G-01 Polypropylene Homopolymer Grade H19G-01 is a polypropylene homopolymers designed for extrusion processing and meet the requirements of the U.S. Food and Drug administration as specified in 12 CFR 177.1520.Applications:Contin.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
Star Plastics ABSFR1 Molding Grade ABSFR Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
Star Plastics ABSFR2 Molding Grade ABS Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
Techmer ES Plastiblend® ABS LG UV Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | 0.125 in, injection molded, unannealed; ASTM D638 |
Styron EMERGEâ„¢ 5710 Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ ABS 5710 advanced resin is an ignition resistant ABS resin with an excellent balance of flow and impact strength. Applications: Monitor Enclosures Surge Protectors and UPS Enclosures .. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
A. Schulman PP 3486-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application.ApplicationThis product is for injection molded applic.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
A. Schulman PP 3486-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application.ApplicationThis product is for injection molded applic.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
A. Schulman PP 3486-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application.ApplicationThis product is for injection molded applic.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 5143C Homopolymer Polypropylene Homopolymer for Extrusion Sheet and Thermoforming Applications Formolene® 5143C is a polypropylene homopolymer designed for sheet and thermoforming applications, which require exceptional clarity. .. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | 2" (50mm) per min; ASTM D638 |
Formosa Plastics Formolene® 5143H Homopolymer Polypropylene Hopolymer Formolene® 5143H is a polypropylene homopolymer designed for sheet and thermoforming applications requiring good clarity. It contains a unique combination of stabilizers, nucleators and a.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
A. Schulman PP 3486-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application.ApplicationThis product is for injection molded applic.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
A. Schulman PP 3486-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application.ApplicationThis product is for injection molded applic.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
A. Schulman PP 3486-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3486-01 is a special homopolymer polypropylene designed with long term heat aging formula for appliance application.ApplicationThis product is for injection molded applic.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 3501 SHF Description: Super High FlowInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 9500B Description: Blow Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 9501 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 9502 Description: Injection Molding Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ABS 9502E Description: Extrusion Grade, Ultra High ImpactInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D-638 |
Axiall CL-7049 Rigid PVC, Molding Georgia Gulf CL-7049 is a clear, high impact vinyl compound formulated for medical and food contact uses.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH034EV Polypropylene, Homopolymer, Fiber, Tape, UV COPYLENE™ CH034EV is a polypropylene homopolymer resin designed for fiber applications. Applications: Filament Yarn, Geotextile & agriculture. Equivalent to Pro-fax® HL348JInformation provided by .. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | 2 in/min; ASTM D638 |
Phillips 66 COPYLENE® CH034W Polypropylene, Homopolymer, Slit Film, LWCO COPYLENE™ CH034W is a medium flow polypropylene homopolymer resin suitable for general injection molding or extrusion applications. Applications: Housewares, Raffia/tapes/strapping. Equivalent to P.. |
|||
Tensile Strength, Yield | 36.5 MPa | 5300 psi | ASTM D638 |
Polymer Resources PPX-GP4-WR Modified PPO, Wear Resistant with HDT of 215 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |