Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Radici Radilon® CS38FL (dry) Copolyamide 6 semiaromatic

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Film Grade
Manufacturer Radici Group Plastics
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® CS38FL (dry) Copolyamide 6 semiaromatic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Film gradeInformation provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527-1/2
Elongation at Break >= 50 %
>= 50 %
ISO 527-1/2
Elongation at Yield 4.1 %
4.1 %
ISO 524-1/2
Tensile Modulus 2.80 GPa
406 ksi
ISO 527-1/2
Flexural Strength 95.0 MPa
13800 psi
ISO 178
Flexural Modulus 2.20 GPa
319 ksi
ISO 178
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 210 °C
410 °F
ISO 1135 7-1-3
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ISO 75/2Af
Vicat Softening Point 70.0 °C
158 °F
ISO 306
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in