Radici Radilon® A RV300R (dry) Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Radici Group Plastics
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Radici Radilon® A RV300R (dry) Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information provided by Radici group.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
Water Absorption 7.0 %
7.0 %
Moisture Absorption at Equilibrium 1.7 %
1.7 %
Viscosity Measurement 145
145
cm³/g Viscosity Number
Mechanical Properties Metric English Comments
Tensile Strength at Break 185 MPa
26800 psi
Elongation at Break 3.6 %
3.6 %
Tensile Modulus 9.70 GPa
1410 ksi
Charpy Impact Unnotched 7.50 J/cm²

@Temperature -30.0 °C
35.7 ft-lb/in²

@Temperature -22.0 °F
8.50 J/cm²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 1.20 J/cm²

@Temperature -30.0 °C
5.71 ft-lb/in²

@Temperature -22.0 °F
1.30 J/cm²

@Temperature 23.0 °C
6.19 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
Vicat Softening Point 245 °C

@Load 5.10 kg
473 °F

@Load 11.2 lb
50°C/h
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+11 ohm-cm
>= 1.00e+11 ohm-cm