Momentive Performance Materials Sanitary 1700â„¢ Construction Sealant

Category Polymer , Adhesive , Thermoset , Silicone , Silicone, RTV, Construction Grade
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name Sanitary 1700™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials Sanitary 1700â„¢ Construction Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
One-part, mildew-resistant sealant for ceramic tile, showers, tubs, and plumbing fixtures. Cure Method: Acetoxy. Tack-free time
Mechanical Properties Metric English Comments
Hardness, Shore A 31
31
ASTM D2240
Tensile Strength, Ultimate 2.80 MPa
406 psi
ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Elasticity is retained to this temperature.
Minimum Service Temperature, Air -62.0 °C
-79.6 °F
Elasticity is retained to this temperature.
Processing Properties Metric English Comments
Processing Temperature 27.0 °C
80.6 °F
Cure time to 0.38 in. is 5-7 days