Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -20.0 °C |
40.4 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT N 32 B PA6 Basic type PA 6 for compounding, for general use. Delivered in the natural mode and in the full RAL color scale.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom PLASTAMID® 6 BT PA6 Basic type PA 6 for compounding, modified for general use. Use: automotive, engineering, electrical and consumer-goods industry. Delivered in natural as well as full RAL color scale.Information Prov.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -20.0 °C |
40.4 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 40 Polyamide 6, 40% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 40% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -20.0 °C |
40.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 GF 50 LS PA6, 50% glass fibre, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6 GF 35 LS PA6 reinforced with glass fiber, UV stabilized PA 6 for injection molding, reinforced with 35% glass fiber, UV stabilized, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B1 GF 6 HML PBT, 6% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -20.0 °C |
40.4 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVALEN PC 93 T 30 PP reinforced with 30% mineral filler Features: Modified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furni.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 30 Polyamide 6, 30% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -20.0 °C |
40.4 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 GF 50 Polyamide 6, 50% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVASTER® B1 GF 6 PBT, 6% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) Zytel® 73G30HSL BK261 is a 30% glass fiber reinforced, heat stabilized, lubricated, black polyamide 6 for injection molding. It has excellent surface appearance and gloss.Information provided by Du.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6
(Unverified Data**) Zytel® BM73G15THS is a 15% glass fiber reinforced, heat stabilized, lubricated, toughened polyamide 6 for blow molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179-1eU |
Gromax BFG30-FH00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® AKV 30 HR H2.0 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis stabilized, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eU |
Lanxess Durethan® AKV 35 HR H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 35% glass fibers, injection molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 130 H2.0 901510 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer-modified, electroplateable, improved notched impact strength and energy absorption under biaxial impact load, good heat-ageing resistance |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
d.a.m.; ISO 179-1eU |
Lanxess Durethan® BKV 40 H2.0 901510 Nylon 6, Glass Fiber Reinforced PA 6, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Solvay TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, DRY Description: TECHNYL® eXten D 218 V30 is a 30% Glass Fiber reinforced and heat stabilized product suitable to the manufacturing of all injection molded parts. This material is available in black... |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Stanyl® TE351 PA46 FR(17) Flame Retardant, Heat Stabilized |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.4 ft-lb/in² @Temperature -22.0 °F |
Edgew 80x10x4 sp=62; ISO 179/1eU |
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® N2720 M210 POM Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature 23.0 °C |
40.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Charpy Impact Unnotched | 8.50 J/cm² @Temperature -30.0 °C |
40.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, Conditioned Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |